C% | Si% | Mn% | P% | S% | Cu% | Cr% | Ni% | Mo% | Al% | V% | Ti% | Zr% |
---|---|---|---|---|---|---|---|---|---|---|---|---|
0,060 | 0,45 | 1,50 | < 0,010 | < 0,010 | < 0,25 | < 0,15 | 1,70 | 0,40 | < 0,050 | < 0,030 | < 0,030 | < 0,030 |
Rm | Rs | Al | Kv |
---|---|---|---|
N/mm² | N/mm² | %5d | -50°C |
760 | 660 | 22 | 75 J |
Protection | MIG: Argon/2% O2 / TIG: I1 (Argon) |
Current and polarity | MIG: DC+ / TIG: DC- |
Welding positions | EN ISO 6947: PA, PB, PC, PD, PE, PF, PG |
Pre Heating temperature | 135 - 165° C |
Interpass temperature | 135 - 165° C |
Post Welding Heat Treatment | as welded |
MIG (mm) | 0,60 - 0,80 - 0,90 - 1,00 - 1,14 - 1,20 - 1,40 - 1,60 |
TIG (mm) | 1,00 - 1,20 - 1,60 - 2,00 - 2,40 - 3,00 - 3,20 - 4,00 |
Base materials to be welded | HY 80; HY 100; Weldox 700; N-A-XTRA 65-70; S690 Q, S460 N; BH 65; BH 70; Hardox; T1; T1A, T1B, HY90; StE460 ; StE690, StE620 |
Applications | NiCrMo alloyed steel with high yeld strength for low temperature. Shipbuilding sector, structural work, industrial equiment, petrolchemical and building industry, cranes, ground movement, tanks, materials handling. |
Approvals | Contact ITALFIL |