CM
LOW ALLOYED WELDING WIRES
SFA-AWS A5.28 ER80S-G
EN ISO 21952-A- G CrMo1Si
EN ISO 21952-A- W CrMo1Si
Average Chemical analysis
C% |
Si% |
Mn% |
P% |
S% | Cu% | Cr% | Ni% | Mo% | Al% | V% | Zr+Ti% | Nb% |
0,090 |
0,65 | 1,05 |
< 0,012 | < 0,015 |
< 0,25 | 1,15 |
< 0,15 | 0,50 |
< 0,020 | < 0,030 |
< 0,15 |
< 0,010 |
The copper value include the surface coating
Typical mechanical properties of all-weld metal
Rm |
Rs |
Al |
Kv |
N/mm² |
N/mm² |
%5d |
+20°C |
630 |
520 | 23 |
100 J |
The mechanical properties are approximate and may range on the basis of the Heat, shielding gas, welding parameters and other factors
Welding process
Protection |
MIG: C1, M21 and similar/ TIG: I1 (Argon) |
Current and polarity |
MIG: DC+ / TIG: DC- |
Welding positions |
EN ISO 6947: PA, PB, PC, PD, PE, PF, PG |
Dimensions
MIG (mm) |
0,60 - 0,80 - 0,90 - 1,00 - 1,14 - 1,20 - 1,40 - 1,60 |
TIG (mm) |
1,00 - 1,20 - 1,60 - 2,00 - 2,40 - 3,00 - 3,20 - 4,00 |
Base materials to be welded |
13CrMo4-5, 15CrMo5, 16CrMoV4, G17CrMo5-5, G22CrMo5-4 A193 Gr.B7, A355 P11-12, A193: B7 13CrMo4-5, 15CrMo3, 13CrMo44, 15CrMo3, 13CrMo4 2, GS-25CrMo 4, GS-17CrMo55, GS17CrMo55, GS22CrMo4 H IV, 15CrMo3, 13CrMoV42, 13CrMo44, St44KL |
Applications |
For heat resistant steels. It grants good resistance to hydrogen and sulphured agents attack. Used for steam boilers, pressure tanks, pipelines, cranes, ground moving machines, presses, chemical and petrolchemical industry. |
Approvals |
Contact ITALFIL |