B3
LOW ALLOYED WELDING WIRES
SFA-AWS A5.28 ER 90S-B3
EN ISO 21952-B- 2C1M
Average Chemical analysis
C% |
Si% |
Mn% |
P% |
S% | Cu% | Cr% | Ni% | Mo% | Al% | V% | FX ppm |
0,080 |
0,50 | 0,60 |
< 0,012 | < 0,015 |
< 0,25 | 2,40 |
< 0,20 | 1,00 |
< 0,020 | < 0,010 |
< 15 |
The copper value include the surface coating
Typical mechanical properties of all-weld metal
Rm |
Rs |
Al |
Kv |
N/mm² |
N/mm² |
%5d |
-10°C |
640 |
540 | 22 |
90 J |
The mechanical properties are approximate and may range on the basis of the Heat, shielding gas, welding parameters and other factors
Welding process
Protection |
MIG: Argon/ 1-5% O2/ TIG: I1 (Argon) |
Current and polarity |
MIG: DC+ / TIG: DC- |
Welding positions |
EN ISO 6947: PA, PB, PC, PD, PE, PF, PG |
Pre Heating temperature |
185-215° C |
Interpass temperature |
185-215° C |
Post Welding Heat Treatment |
690 ± 15° C |
Dimensions
MIG (mm) |
0,60 - 0,80 - 0,90 - 1,00 - 1,14 - 1,20 - 1,40 - 1,60 |
TIG (mm) |
1,00 - 1,20 - 1,60 - 2,00 - 2,40 - 3,00 - 3,20 - 4,00 |
Base materials to be welded |
10CrMo9-10, GS 17CrMoV5 11, 10CrSiMoV7, 12CrSiMo8, GS12CrMo9 10, 10CrSiMoV7, 10Cr V63, 12CrSiMo8 |
Applications |
Cr-Mo alloyed steels resistant to high temperatures, corrosion and attack of sulphured agents. Boilers, pipelines, steam boilers, pressure tanks, oil industry, thermoelectrical industry, chemical and petrolchemical industry. |