MO
LOW ALLOYED WELDING WIRES
SFA-AWS A5.28 ER70S-A1
EN ISO 14341-A- G 2Mo
EN ISO 21952-A- G/W MoSi
EN ISO 636-A- W 2Mo
Average Chemical analysis
C% |
Si% |
Mn% |
P% |
S% | Cu% | Cr% | Ni% | Mo% | Al% | V% | Zr+Ti% |
0,090 |
0,60 | 1,20 |
< 0,015 | < 0,015 |
< 0,25 | < 0,15 |
< 0,10 | 0,50 |
< 0,030 | < 0,020 |
< 0,050 |
The copper value include the surface coating
Typical mechanical properties of all-weld metal
Rm |
Rs |
Al |
Kv |
Kv |
N/mm² |
N/mm² |
%5d |
+20°C |
-40°C |
610 |
520 | 25 |
150 J |
> 47 J |
The mechanical properties are approximate and may range on the basis of the Heat, shielding gas, welding parameters and other factors
Welding process
Protection |
MIG: C1, M21, Argon + 1-5% O2,/ TIG: I1 (Argon) |
Current and polarity |
MIG: DC+ / TIG: DC- |
Welding positions |
EN ISO 6947: PA, PB, PC, PD, PE, PF, PG |
Pre Heating temperature |
135-165° C |
Interpass temperature |
135-165° C |
Post Welding Heat Treatment |
620 ± 15° C |
Dimensions
MIG (mm) |
0,60 - 0,80 - 0,90 - 1,00 - 1,14 - 1,20 - 1,40 - 1,60 |
TIG (mm) |
1,00 - 1,20 - 1,60 - 2,00 - 2,40 - 3,00 - 3,20 - 4,00 |
Base materials to be welded |
P295GH, P355GH, 16Mo3, 17Mo3, 14Mo6, S275, S355, S420, A210, A285, A335, A516, S275Ml, S355M, S420M, S460 15Mo3, 10MnMo45, 11MnMo45, GS60, GS22Mo4, 20MnMoNi5-5, 15NiCuMoNd5S, 17MnMoV64 |
Applications |
Structural steels resistant to heat and to hot work creep. Pipelines, steam boilers, pressure tanks, gas pipes, ship building sector, chemical, petrolchemical sector, equipment, building of cranes. |
Approvals |